Pressure Effect on the Thermal Runaway Behaviors of Lithium-Ion Battery ...
The high temperature inside the battery leads to the melting of the battery separator, a large-area internal short circuit occurs in the battery, and the battery voltage drops sharply. Stage III When the battery surface temperature gets to T TR, the battery surface temperature begins to rise exponentially and reaches T max instantly [ 19 ].